I just got done making these from a mix of 308 brass, mil brass to be precise. I've made these in the past for folks and towards the end they all worked just great. These have gone through 2 different sizing operations, 2 different lathe operations, and have been reamed to the point all you boolit users wont have a problem.
These do take some time to make from 308 brass, almost as much when I make the 25 or 32Rem cases. These aren't going to be what a person would call cheap, but these are about as perfect as a persons going to get.
The 1 thing I didn't do is make the extraction groove smaller. And I mean by .005 than what they are now. Only reason I bring this up is if someone has a shell holder made just for the 35Rem cases, the cases wont work because of it, but work just fine if you use a shell holder for the 308 cases. I would have to charge more than what I'm offering these for and I want to keep the cost down for these. And yes they've been annealed and primer crimp removed.
Note: These are heavier cases, work your loads up and never start near max load data. And with proper care these should last a good long time.
These will have all the work done to them to the point you just load them up and go bang.
Link with pictures:
http://castboolits.gunloads.com/showthread.php?238582-35-Remington-Brass-from-308-1x-fired-Mil-brassThese are .50ea plus ship regardless of how many