It's been a long process, but it all came together today. I originally got free lead that was taken out of an X-ray room. I decided it was time to get into casting. I build my PID controller. Bought a Lee pot, pewter, and linotype. Melted the lead down to ingots today. Weighed out some and remelted with linotype and pewter to give me a 95% lead, 3% antimony, and 2% tin. Used that alloy to cast my .356 95gr bullets for my 380. What do you all think? My only issue was out of the 6 cavities there was almost always 1 or 2 that the base didn't completely fill. Typically one of the inner cavities. I was casting at 700*.