Quote
I'm thinking I let the blocks get too hot and the alloy was flowing too fast because the problem started at the bottom of the pour.


Not very experienced here, but when my Lee molds shearing starts to have a smear, I just slow down my cycle. Let it cool just a hair between fills. Works for me. miles