Was checking dims on LR brass a short while back and it is quite variable. Most US production has a case wall of .008" at the mouth and foreign manufacture runs .007". That's a ~12.5% spread in case weight on the face of it, but there are other aspects at play I did not measure.


I am..........disturbed.