What can I do with a "frosty" action that has some pitting. It's not worth filling it in with weld or anything else like that. Is there one finish that hides better than another? I have bead blasted it and can not seem to blend the pitting. It is an otherwise nice FN 24/47 action. It is gonna be a "utilitarian" grade shooter when I'm done with it. I'm considering Gunskins. I'll try to get pix up.