Casting a few of these for the first time today. Was a little tricky to get the nose right.. needed a bit more tin and slightly warmer alloy, then it started happening. These are as they dropped from the mold. A little thumbnail action on the nose cleaned it up.

Anyway if anyone has used these for hunting I would be very interested to hear of your results.
These are 12bhn, lead and lino (3:1) and tin.