I ended up with five full gallon pots of alloy. By my calcs, that should be pretty close to 100 lb ea. Two pots as low as 10 BHN, one at 15.4, and two more at 14.3 as they came out of the pot.

I have the initial batches distributed among six piles for remelting. The blend should give me just the BHN I desire after blending.

I have 20 lbs of Roto-metals Super Hard and 20 lbs of 40-60 solder left over. Apparently my scrap had a lot more Antimony content than I had guessed. Might have been a good amount of wheel weights in those blocks.


People who choose to brew up their own storms bitch loudest about the rain.