Thanks. I've read over the basics of doing it: degrease, apply compound, boil, let rust, card (may have too many steps or some out of order) and then repeat the process until desired depth of color is reached.

My concerns are: how do you keep the bore from rusting and how do you card (and what do you card with?) the hard-to-reach recesses of small parts and the inside of the receiver?