How about a how-to reference for this salt bath annealing? Sounds similar to "niter bluing" of small steel parts.
Thanks,
Rex
EDIT - never mind...
Salt Bath AnnealingSecond edit: Which led me to:
AMP's responseInteresting stuff. Makes me wonder if my candle method execution is doing it right. Anybody know if such rigorous testing as AMP did has been done on candle annealed cases? I thrust MD's lessons so I'm not worried about it, just curious.