Originally Posted by tzone
Experienced or not, don't let them give you the "hot mix" bullschitt. They didn't get a hot mix, they were too slow for the size of the pour. They needed more labor.

It happened to me last fall on a train station project. Not enough labor and they lost the mix.

I'm very glad they're working with you on it!!!


This ^^^^^

Originally Posted by tzone
Originally Posted by 458 Lott
I'd be more up for the industrial coating vs. a 2" cap. Seems like a thin cap like that would just be asking for trouble down the road.


Bingo!


And this ^^^^

I doubt you could an engineer to sign off on a 2" cap anyway, and I'd dam sure want one before I'd even consider it.

Epoxy and keep rolling at this point.
Luck